September 2025

ORNL Report

Analysis of deformation and fracture mechanisms in the harvested high-dose baffle-former bolt with stress-corrosion cracks formed while in service

By:
Gussev, Maxim N; Kang, Soyoung ; Lach, Timothy G; Chen, Xiang
Publication Date:
September 22, 2025