- By:
- Smith, Jacob G; Kumar, Abinash ; Chi, Miaofang ; Liccardo, Gennaro; Cendejas, Melissa; Mandal, Shyama; Stone, Michael; Porter, Stephen; nhan, Bang; Plessow, Phillip; Cegelsky, Lynette; Osio-Norgaard, Jorge; Abild pedersen, Frank; Datye, Abhaya; Bent, Stacey; Cargnello, Matteo
- Journal Name:
- Journal of the American Chemical Society
- Page Number:
- 23909-23922
- Volume:
- 146
- Issue Number:
- 34
- Publication Date:
- September 5, 2024
- View DOI Listing:
- https://doi.org/10.1021/jacs.4c06423
Abstract
Platinum exhibits desirable catalytic properties, but it is scarce and expensive. Optimizing its use in key applications such as emission control catalysis is important to reduce our reliance on such a rare element. Supported Pt nanoparticles (NPs) used in emission control systems deactivate over time because of particle growth in sintering processes. In this work, we shed light on the stability against sintering of Pt NPs supported on and encapsulated in Al2O3 using a combination of nanocrystal catalysts and atomic layer deposition (ALD) techniques. We find that small amounts of alumina overlayers created by ALD on preformed Pt NPs can stabilize supported Pt catalysts, significantly reducing deactivation caused by sintering, as previously observed by others. Combining theoretical and experimental insights, we correlate this behavior to the decreased propensity of oxidized Pt species to undergo Ostwald ripening phenomena because of the physical barrier imposed by the alumina overlayers. Furthermore, we find that highly stable catalysts can present an abundance of under-coordinated Pt sites after restructuring of both Pt particles and alumina overlayers at a high temperature (800 °C) in C3H6 oxidation conditions. The enhanced stability significantly improves the Pt utilization efficiency after accelerated aging treatments, with encapsulated Pt catalysts reaching reaction rates more than two times greater than those of a control supported Pt catalyst.